Inconel 625 vs Incoloy 825: differences and selection
Inconel 625 (UNS N06625) is a nickel alloy with about 9 % molybdenum plus niobium: mechanically stronger, with a PREN close to 50, for seawater, hot chlorides and high temperature. Incoloy 825 (N08825) is a Ni-Fe-Cr alloy with about 40 % nickel and 30 % iron (Ni 38–46 %, Fe ≥ 22 %), plus copper and titanium: it is the economical choice for sulfuric and phosphoric acid and acidic media with H₂S.
| Property | Inconel 625 / Alloy 625 | Incoloy 825 |
|---|---|---|
| Identification | ||
| Group | Nickel alloys | Nickel alloys |
| UNS | N06625 | N08825 |
| W.Nr. / EN | 2.4856 | 2.4858 – NiCr21Mo |
| Chemical composition (%) | ||
| C | ≤ 0.10 | ≤ 0.05 |
| Mn | ≤ 0.50 | ≤ 1.0 |
| Si | ≤ 0.50 | ≤ 0.5 |
| P | ≤ 0.015 | – |
| S | ≤ 0.015 | ≤ 0.03 |
| Cr | 20.0–23.0 | 19.5 – 23.5 |
| Ni | ≥ 58.0 | 38.0 – 46.0 |
| Mo | 8.0–10.0 | 2.5 – 3.5 |
| Cu | – | 1.5 – 3.0 |
| Fe | ≤ 5.0 | ≥ 22.0 |
| Ti | ≤ 0.40 | 0.6 – 1.2 |
| Nb | 3.15–4.15 (Nb+Ta) | – |
| Al | ≤ 0.40 | ≤ 0.2 |
| Composition: standard | ASTM B443/B444/B446/B564/B704/B705 N06625 | ASTM B425 / B564 (UNS N08825) |
| Mechanical properties (minimum) | ||
| Yield strength | – | – |
| Tensile strength | – | – |
| Elongation | – | – |
| Hardness | – | – |
| Properties: condition | ASTM B564 N06625 annealed, up to 102 mm | annealed (ASTM B564 / B425) |
| Use and supply | ||
| PREN (minimum – typical) | 46 – 51 | 28 – 31 |
| Density | 8.44 g/cm³ | – |
| Service temperature | – | From cryogenic up to ~540 °C (usual limit in ASME pressure vessels). |
| Standards by product form | Forging (flanges, blocks, rings): ASTM B564 / ASME SB-564 Bar and rod: ASTM B446 / ASME SB-446 Plate, sheet and strip: ASTM B443 / ASME SB-443 Seamless tube: ASTM B444 / ASME SB-444 Welded tube and pipe: ASTM B704 (tube) / B705 (pipe); ASME SB-704 / SB-705 | Bar: ASTM B425 Forging: ASTM B564 Plate: ASTM B424 Tube: ASTM B423 and B163 (seamless), B704/B705 (welded) |
| Typical applications | Oil and gas Marine and offshore Chemicals and petrochemicals Aerospace | Well tubing and components with H₂S/CO₂ (oil and gas) Sulfuric and phosphoric acid equipment Pickling tanks, baskets and coils Gas scrubbers (FGD) |
Composition and minimum properties per the standard listed on each datasheet; PREN uses the minimum and the middle of the ranges. For the actual value, use the heat certificate.
Most searched comparisons
- 316 / 316L stainless x 317L stainless steel
- Duplex 2205 (F51 / S31803) x Super duplex 2507 / F53 / S32750
- Duplex 2205 (F51 / S31803) x Duplex S32205 / F60
- 17-4PH stainless steel – UNS S17400 (ASTM A564 Type 630) x 15-5PH – UNS S15500 (XM-12)
- SAE 4140 x SAE 4340
For pitting resistance, see the PREN calculator; for steel weldability, the carbon equivalent; to choose by medium, steel by corrosive medium.
Frequently asked questions
Can 625 replace 825?
In most media, yes, with margin. The switch only does not pay off when 825 already resists, because 625 costs more.
Which one withstands higher temperature?
625, which keeps its strength when hot and is also used at high temperature. 825 is an alloy for aqueous corrosion.
What about cladding and welding?
625 is the most used alloy for weld overlay and as a filler metal (ERNiCrMo-3), including for welding 825.