2507 (UNS S32750, F53) is the super duplex: about 25 % chromium, 3.0–5.0 % molybdenum (typically ≈ 4 %) and more nitrogen than 2205 (S31803/S32205, F51/F60). PREN is 40 or higher (the value required in purchase specs), against 31–34 for 2205, and minimum yield rises from 450 to 550 MPa. Use 2507 in seawater and hot chlorides; 2205 handles moderate chlorides at lower cost.

Duplex 2205 vs super duplex 2507
PropertyDuplex 2205 (F51 / S31803)Super duplex 2507 / F53 / S32750
Identification
GroupDuplexDuplex
UNSS31803S32750
W.Nr. / EN1.44621.4410
Chemical composition (%)
C≤ 0.030≤ 0.030
Mn≤ 2.00≤ 1.20
Si≤ 1.00≤ 0.80
P≤ 0.030≤ 0.035
S≤ 0.020≤ 0.020
Cr21.0–23.024.0–26.0
Ni4.5–6.56.0–8.0
Mo2.5–3.53.0–5.0
N0.08–0.200.24–0.32
Composition: standardUNS S31803 (A240, A182 F51, A790)A240/A182 F53 (S32750)
Mechanical properties (minimum)
Yield strength––
Tensile strength––
Elongation––
Hardness––
Properties: conditionA182 F51 (S31803), solution annealedA182 F53, solution annealed, ≤ 50 mm
Use and supply
PREN (minimum – typical)31 – 3438 – 43
Density7.8 g/cm³7.8 g/cm³
Service temperature––
Standards by product formPlate, coil, strip: A240 / SA-240
Bar and section: A276; A479 / SA-479
Forging and flange: A182 / SA-182
HIP part (powder metallurgy): A988 / SA-988
Seamless and welded pipe (piping): A790 / SA-790
Forging and flange (B16.5): A182 / SA-182
Bar: A479 / SA-479; A276
Plate, coil, strip: A240 / SA-240
Seamless pipe (line): A790 / SA-790
Heat exchanger tube: A789 / SA-789
Typical applicationsOffshore oil and gas
Chemicals and petrochemicals
Pulp and paper
Chemical tankers
Offshore oil and gas
Subsea
Desalination (SWRO)
Chemicals and pulp

Composition and minimum properties per the standard listed on each datasheet; PREN uses the minimum and the middle of the ranges. For the actual value, use the heat certificate.

Quote these materials

Most searched comparisons

For pitting resistance, see the PREN calculator; for steel weldability, the carbon equivalent; to choose by medium, steel by corrosive medium.

Frequently asked questions

Can I replace 2205 with 2507?

Yes, 2507 works wherever 2205 works in corrosion and strength. The opposite does not hold for seawater or hot chlorides.

Do both have the same temperature limit?

Yes. The ASME code limits both to 316 °C (600 °F). In long exposure above ~250–280 °C there is a risk of 475 °C embrittlement (hardening of the ferrite); check the limit in the design code.

What care is needed when welding 2507?

Control heat input and interpass temperature to keep the ferrite–austenite balance, and use a super duplex filler metal (ER2594).

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)