15-5PH (UNS S15500) is a version of 17-4PH (S17400) with less chromium and almost no delta ferrite. Both are precipitation hardened with the same treatments (H900 to H1150) and reach similar strength, but 15-5PH has better transverse toughness and ductility in large sections, which is why it is preferred in aerospace. For shafts, valves and general parts, 17-4PH does the job and is easier to find.

17-4PH vs 15-5PH
Property17-4PH stainless steel – UNS S17400 (ASTM A564 Type 630)15-5PH – UNS S15500 (XM-12)
Identification
GroupStainless steelsStainless steels
UNSS17400S15500
W.Nr. / EN1.4542 (X5CrNiCuNb16-4)1.4545 (X5CrNiCu15-5)
Chemical composition (%)
C≤ 0.07≤ 0.07
Mn≤ 1.00≤ 1.00
Si≤ 1.00≤ 1.00
P≤ 0.040≤ 0.040
S≤ 0.030≤ 0.030
Cr15.0 – 17.514.0 – 15.5
Ni3.0 – 5.03.5 – 5.5
Cu3.0 – 5.02.5 – 4.5
Febalancebalance
Nb0.15 – 0.45 (Nb+Ta)0.15 – 0.45 (Nb+Ta)
Composition: standardASTM A564 Type 630ASTM A564 XM-12
Mechanical properties (minimum)
Yield strength––
Tensile strength––
Elongation––
Hardness––
Properties: conditionAged – ASTM A564 minimums (bar); see the aging tableAged – ASTM A564 minimums (bar, longitudinal); other conditions in the aging table
Use and supply
PREN (minimum – typical)15 – 1614 – 15
Density––
Service temperatureUp to ≈ 315 °C; above that, prolonged exposure embrittles (loss of toughness).Up to ≈ 315 °C; prolonged exposure above that causes embrittlement (475 °C aging).
Standards by product formBar: ASTM A564 Type 630; AMS 5643; AMS 5622 (VAR)
Forging: ASTM A705 Type 630; AMS 5643
Plate: ASTM A693 Type 630; AMS 5604
Casting: ASTM A747 CB7Cu-1
H2S service: NACE MR0175/ISO 15156 (H1150D, ≤ 33 HRC)
Bar: ASTM A564 XM-12; AMS 5659
Forging: ASTM A705 XM-12; AMS 5659
Plate: ASTM A693 XM-12; AMS 5862
Equivalent casting: ASTM A747 CB7Cu-2
Typical applicationsPump and propeller shafts
Valve stems and internals
Aircraft hardware and fittings
Studs, bolts and couplings
Aircraft structures and fittings
Shafts and valve stems
Pump and compressor components
Gears and couplings

Composition and minimum properties per the standard listed on each datasheet; PREN uses the minimum and the middle of the ranges. For the actual value, use the heat certificate.

Quote these materials

Most searched comparisons

For pitting resistance, see the PREN calculator; for steel weldability, the carbon equivalent; to choose by medium, steel by corrosive medium.

Frequently asked questions

Is the heat treatment the same?

Yes. Both are solution annealed (condition A) and aged at the same temperatures; the H condition sets strength and hardness.

Which one has better corrosion resistance?

They are similar, around that of a 304. Neither is suited to stagnant seawater.

Can I replace 17-4PH with 15-5PH?

Generally yes, in the same H condition. Check the drawing: aerospace and some customers require the specific standard (for example AMS 5659 for 15-5PH).

HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)