Inconel 625 与 Incoloy 825 对比:区别及选择
Inconel 625(UNS N06625)是镍基合金,含约 9 % 的钼和铌:力学强度更高,PREN 接近 50,适用于海水、高温氯化物和高温环境。Incoloy 825(N08825)是 Ni-Fe-Cr 合金,含约 40 % 镍和 30 % 铁(Ni 38–46 %,Fe ≥ 22 %),另含铜和钛:是硫酸、磷酸及含 H₂S 酸性介质的经济之选。
| 性能 | Inconel 625 / Alloy 625 | Incoloy 825 |
|---|---|---|
| 标识 | ||
| 组别 | 镍合金 | 镍合金 |
| UNS | N06625 | N08825 |
| W.Nr. / EN | 2.4856 | 2.4858 – NiCr21Mo |
| 化学成分 (%) | ||
| C | ≤ 0.10 | ≤ 0.05 |
| Mn | ≤ 0.50 | ≤ 1.0 |
| Si | ≤ 0.50 | ≤ 0.5 |
| P | ≤ 0.015 | – |
| S | ≤ 0.015 | ≤ 0.03 |
| Cr | 20.0–23.0 | 19.5 – 23.5 |
| Ni | ≥ 58.0 | 38.0 – 46.0 |
| Mo | 8.0–10.0 | 2.5 – 3.5 |
| Cu | – | 1.5 – 3.0 |
| Fe | ≤ 5.0 | ≥ 22.0 |
| Ti | ≤ 0.40 | 0.6 – 1.2 |
| Nb | 3.15–4.15 (Nb+Ta) | – |
| Al | ≤ 0.40 | ≤ 0.2 |
| 成分:标准 | ASTM B443/B444/B446/B564/B704/B705 N06625 | ASTM B425 / B564 (UNS N08825) |
| 力学性能(最低值) | ||
| 屈服强度 | – | – |
| 抗拉强度 | – | – |
| 伸长率 | – | – |
| 硬度 | – | – |
| 性能:状态 | ASTM B564 N06625 退火,最大102 mm | 退火态(ASTM B564 / B425) |
| 用途与供货 | ||
| PREN(最低 – 典型) | 46 – 51 | 28 – 31 |
| 密度 | 8.44 g/cm³ | – |
| 使用温度 | – | 从低温直至约540 °C(ASME压力容器的常用上限)。不适用于蠕变工况。 |
| 按产品形式的标准 | 锻件(法兰、锻块、环件): ASTM B564 / ASME SB-564 棒材与线材: ASTM B446 / ASME SB-446 板、薄板与带材: ASTM B443 / ASME SB-443 无缝管: ASTM B444 / ASME SB-444 焊接管: ASTM B704(管)/ B705(管道);ASME SB-704 / SB-705 | 棒材: ASTM B425 锻件: ASTM B564 板材: ASTM B424 管材: ASTM B423 和 B163(无缝)、B704/B705(焊接) |
| 典型应用 | 石油和天然气 船舶与海洋 化工与石化 航空航天 | 含H₂S/CO₂的油井油管及部件(油气) 硫酸和磷酸设备 酸洗槽、吊篮和盘管 烟气脱硫洗涤塔(FGD) |
成分和最低性能依据各技术资料所列标准;PREN 采用范围的最低值和中值。实际数值请以炉号证书为准。
热门对比
常见问题
625 能替代 825 吗?
在大多数介质中可以,而且余量充足。只有当 825 已能耐受时才不划算,因为 625 价格更高。
哪种耐温更高?
625,它在高温下保持强度,也用于高温工况。825 是用于水溶液腐蚀的合金。
堆焊和焊接呢?
625 是堆焊(overlay)最常用的合金,也是常用焊材(ERNiCrMo-3),包括用于焊接 825。