Special alloys for refining and petrochemicals

In refining, temperature, hydrogen and sulfur rule. Chromium-molybdenum steels (F11, F22, F5, F9, F91) are chosen by the Nelson curves of API RP 941 for high-temperature hydrogen. 321 and 347 stainless avoid sensitization, and Incoloy 800HT serves high-temperature furnaces.

Technical review Oct 2026

Conditions and recommended alloys

Typical refining and petrochemical conditions and alloys used
Application or mediumWhat attacks the partAlloys used
High-temperature hydrogen (hydrotreating)High-temperature hydrogen attack (HTHA), per API RP 941ASTM A182 F22 / P22 (2¼Cr-1Mo), ASTM A182 F5, ASTM A182 F9, ASTM A182 F91 Type 1
Crude with sulfur and naphthenic acidsSulfidation and naphthenic acid corrosionASTM A182 F5, ASTM A182 F9, 316 / 316L stainless, 317L stainless steel
Shutdowns of units with stainless steelIntergranular cracking by polythionic acids321 stainless steel, 347 stainless steel
Furnaces and radiant tubesOxidation, carburization and creepIncoloy 800HT, 310S stainless steel, Inconel 601

The table is a guide. To compare alloys in a defined medium, concentration and temperature, use the steel by corrosive medium selector and the PREN calculator.

Industry standards and requirements

  • API RP 941: steels for high-temperature hydrogen (Nelson curves).
  • API RP 571: damage mechanisms in refineries.
  • API 530: calculation of furnace tubes.
  • NACE SP0170: protection of stainless steel against polythionic acids during shutdowns.
  • ASME B31.3 and B16.5: process piping and flanges.

Parts we supply for refining and petrochemicals

Flanges, forged nozzles, rings, pipes and plates. We forge, cut and machine to your drawing, with a 3.1 certificate. See parts and equipment · See services

Catalog materials used in refining and petrochemicals

Frequently asked questions

What is the difference between F22 and F91?

F22 is a 2¼Cr-1Mo steel. F91 has 9 % chromium, 1 % molybdenum and vanadium, with much higher creep strength: at high temperature, it allows a thinner wall.

321 or 347?

Both are stabilized stainless steels that do not sensitize in the 425 to 815 °C range: 321 with titanium and 347 with niobium. 347 is usually preferred for welded parts, because less niobium is lost in welding.

What certificate do you deliver with?

With the mill's 3.1 inspection certificate (EN 10204), showing heat, chemical composition and mechanical properties. Extra tests, such as PMI, ultrasonic and hardness, are included in the quote when the project requires them.

Other industries

Need the right alloy for refining and petrochemicals?Tell us the application, the medium and the temperature. We recommend the alloy and quote with a 3.1 certificate.
Request a quoteWhatsApp
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)